MicroChemicals Silicon, Quartz, Glass and Fused Silica Wafer Stock List (Revised: 16.05.2024 19:11 MEZ)


Other wafer types (also cut wafer pieces) and technical details on request: info@microchemicals.eu
       
 1 Inch2 Inch3 Inch4 Inch5 Inch6 Inch8 Inch12 InchStücke
CZ-Si4095 Wafer7600 Wafer11704 Wafer18860 Wafer749 Wafer13067 Wafer5277 Wafer724 Wafer2817 Wafer
FZ-Si0 Wafer1317 Wafer723 Wafer3043 Wafer0 Wafer601 Wafer0 Wafer0 Wafer0 Wafer
Si+SiO20 Wafer1339 Wafer1084 Wafer4771 Wafer0 Wafer403 Wafer0 Wafer0 Wafer1552 Wafer
Si+SiNx0 Wafer0 Wafer130 Wafer514 Wafer0 Wafer0 Wafer0 Wafer0 Wafer0 Wafer
Quartz200 Wafer77 Wafer202 Wafer168 Wafer0 Wafer0 Wafer0 Wafer0 Wafer306 Wafer
Fused Silica750 Wafer5016 Wafer503 Wafer1828 Wafer0 Wafer492 Wafer26 Wafer0 Wafer20509 Wafer
Glass200 Wafer785 Wafer689 Wafer1714 Wafer0 Wafer425 Wafer58 Wafer0 Wafer3342 Wafer

1 Inch Silicon, Quartz, Fused Silica and Glass Wafers
Qual.MaterialSize
(inch)
Orien-
tation
PolishedThick-
ness (μm)
DopingResistivity
(ohm cm)
Coating# available
now1/soon2
Article Number
(WebShop)
Borosilicate1###double-side250 ± 25 200 / 200WGS10250250XXXXXXNN1
Quartz1Z-Cutdouble-side500 ± 20 200 / 200WQC10500200X0000XNN1
PrimeCZ-Si1(100)double-side150 ± 25Boron0.008 - 0.02 155 / 155WSA10150250B8021XNN1
PrimeCZ-Si1(100)double-side200 ± 25Boron1 - 10 197 / 197WSA10200250B1314XNN1
PrimeCZ-Si1(100)double-side280 ± 25Boron1 - 10 609 / 609WSA10280250B1314XNN1
PrimeCZ-Si1(100)one-side275 ± 25Boron1 - 20 200 / 200WSD10275250B1324XNN1
PrimeCZ-Si1(100)one-side280 ± 25Arsenic0.001 - 0.005 441 / 441WSD10280250A1050SNN1
PrimeCZ-Si1(100)one-side280 ± 25Boron0.001 - 0.05 1254 / 1254WSD10280250B1051XNN1
PrimeCZ-Si1(100)one-side280 ± 25Boron1 - 20 219 / 219WSD10280250B1324SNN1
PrimeCZ-Si1(100)one-side625 ± 25Boron1 - 20 458 / 458WSD10625250B1324XNN1
Dummy3CZ-Si1(100)one-side275 ± 25Boron1 - 20 337 / 337WSV10275250B1324XNN1
Dummy3CZ-Si1(100)one-side2500 ± 50Boron1 - 10 225 / 225WSV12500500B1314XNN1
Fused Silica1###double-side500 ± 25 75 / 75WUS10500250X0000SNN1
Fused Silica1###double-side500 ± 25 150 / 675WUS10500250X0000XNN1
Interested in an offer? Please send us an e-mail with the article numbers(s) (20-digit code in the right column of the table above) and number to info@microchemicals.com
2 Inch Silicon, Quartz, Fused Silica and Glass Wafers
Qual.MaterialSize
(inch)
Orien-
tation
PolishedThick-
ness (μm)
DopingResistivity
(ohm cm)
Coating# available
now1/soon2
Article Number
(WebShop)
PrimeFZ-Si2(100)double-side280 ± 1010000 - 100000 35 / 235WFA20280100X1718XNN1
PrimeFZ-Si2(100)double-side500 ± 15Boron1000 - 100000 125 / 125WFA20500150B1618SNN1
PrimeFZ-Si2(100)double-side500 ± 15Phosphor1000 - 100000 139 / 139WFA20500150P1618SNN1
PrimeFZ-Si2(100)double-side1500 ± 25Boron3000 - 100000 149 / 149WFA21500250B3618SNN1
PrimeFZ-Si2(100)one-side280 ± 2510000 - 1000000 110 / 110WFD20280250X1719XNN1
PrimeFZ-Si2(100)one-side300 ± 105000 - 1000000 221 / 221WFD20300105X5619SNN2
PrimeFZ-Si2(100)one-side1600 ± 25Boron3000 - 3000 20 / 20WFD21600250B3638SNN1
PrimeFZ-Si2(100)one-side1600 ± 25Phosphor3000 - 3000 27 / 27WFD21600250P3638SNN1
PrimeFZ-Si2(111)one-side415 ± 1510000 - 100000 91 / 91WFF20415150X1718XNN1
Borosilicate2###double-side500 ± 25 75 / 75WGS2050025XX0000SNN1
Borosilicate2###double-side500 ± 25 588 / 588WGS2050025XX0000SNN2
Borosilicate2###double-side2000 ± 25 90 / 90WGS22000250X0000SNN1
Borosilicate2###double-side2000 ± 25 32 / 32WGS22000250X0000SNN2
Quartz2Y-Cutdouble-side200 ± 25 27 / 27WQB20200250X0000SNN1
Quartz2ST-Cutdouble-side700 ± 25 50 / 50WQL20700250XXXXXSNN1
PrimeCZ-Si2(100)double-side200 ± 10Boron1 - 10 73 / 73WSA20200105B1314SNN1
PrimeCZ-Si2(100)double-side279 ± 20Boron1 - 10 389 / 389WSA20279200B1314SNN1
PrimeCZ-Si2(100)double-side500 ± 15Boron1 - 10 5 / 205WSA20500150B1314SNN1
PrimeCZ-Si2(100)double-side500 ± 15Phosphor1 - 10 100 / 100WSA20500150P1314SNN1
PrimeCZ-Si2(100)one-side279 ± 20Phosphor1 - 10 825 / 825WSD20279200P1314SNN1
PrimeCZ-Si2(100)one-side280 ± 15Arsenic0.001 - 0.005 11 / 311WSD20280150A1050SNN1
PrimeCZ-Si2(100)one-side280 ± 25Boron1 - 10 299 / 799WSD20280250B1314SNN1
PrimeCZ-Si2(100)one-side400 ± 25Phosphor10 - 20 175 / 175WSD20400250P1424SNN1
PrimeCZ-Si2(100)one-side500 ± 25Boron1 - 10 315 / 315WSD20500250B1314SNN1
PrimeCZ-Si2(100)one-side2000 ± 25Boron1 - 20 75 / 75WSD22000250B1324SNN1
PrimeCZ-Si2(100)one-side3000 ± 25Arsenic0.001 - 0.005 44 / 44WSD23000250A1050SNN2
PrimeCZ-Si2(111)one-side400 ± 25Arsenic0.001 - 0.005 279 / 279WSF20400250A1050SNN1
PrimeCZ-Si2(111)one-side400 ± 25Phosphor10 - 20 75 / 75WSF20400250P1424SNN1
PrimeCZ-Si2(111)one-side500 ± 15Boron1 - 10 103 / 103WSF20500150B1314SNN1
TestCZ-Si2(100)one-side279 ± 25Boron1 - 20 1150 / 1150WSM20279250B1324SNN1
TestCZ-Si2(100)one-side500 ± 15Boron1 - 20 625 / 625WSM20500150B1324SNN1
Dummy3CZ-Si2(100)one-side500 ± 50Boron0.001 - 100 2000 / 2000WSV20500500B1015XNN2
PrimeSi + SiO2 (dry)2(100)one-side279 ± 20Boron0.001 - 0.0550 nm275 / 275WTD20279200B1051S051
PrimeSi + SiO2 (dry)2(100)one-side279 ± 20Boron1 - 10100 nm191 / 191WTD20279200B1314S101
PrimeSi + SiO2 (dry)2(100)one-side280 ± 20Boron0.001 - 0.0550 nm139 / 139WTD20280200B1051S051
Fused Silica2###double-side200 ± 25 66 / 66WUA20200250X0000SNN1
Fused Silica2###double-side380 ± 25 190 / 190WUS20380250X0000XNN1
Fused Silica2###double-side500 ± 25 100 / 100WUS20500250X0000SNN1
Fused Silica2###double-side500 ± 25 90 / 1090WUS20500250X0000SNN2
Fused Silica2###double-side500 ± 25 559 / 559WUS20500250X0000XNN1
Fused Silica2###double-side500 ± 25 1718 / 1718WUS20500250XXXXXSNN1
Fused Silica2###double-side700 ± 25 1025 / 1025WUS20700250X0000XNN1
Fused Silica2###double-side1000 ± 25 250 / 250WUS21000250X0000XNN1
Fused Silica2###double-side3000 ± 50 14 / 14WUS2300050XXXXXXXNN1
Fused Silica2###double-side3600 ± 50 4 / 4WUS23600500X0000XNN1
PrimeSi + SiO2 (wet)2(100)one-side279 ± 20Boron1 - 10300 nm264 / 264WWD20279200B1314S301
PrimeSi + SiO2 (wet)2(100)one-side279 ± 25Boron1 - 10500 nm295 / 295WWD20279250B1314S501
PrimeSi + SiO2 (wet)2(100)one-side279 ± 251000 - 100000250 nm0 / 175WWD20279250X1618S251
PrimeCZ-Si2(100)none270 ± 20Boron0 - 0.05 0 / 1(5)WSG20270200B0051SNN#
PrimeCZ-Si2(100)one-side1000 ± 25Boron1 - 10 0 / 18(5)WSD21000250B1314SNN#
PrimeCZ-Si2(111)one-side500 ± 15Boron1 - 10 0 / 100(5)WSF20500150B1314SNN#
PrimeCZ-Si2(100)one-side500 ± 15Boron1 - 10 0 / 25(5)WSD20500150B1314SNN#
PrimeFZ-Si2(100)one-side300 ± 25Phosphor5000 - 1000000 0 / 100(5)WFD20300255P5619SNN#
PrimeFZ-Si2(111)one-side400 ± 155000 - 1000000 0 / 100(5)WFF20400150X5619SNN#
Interested in an offer? Please send us an e-mail with the article numbers(s) (20-digit code in the right column of the table above) and number to info@microchemicals.com
3 Inch Silicon, Quartz, Fused Silica and Glass Wafers
Qual.MaterialSize
(inch)
Orien-
tation
PolishedThick-
ness (μm)
DopingResistivity
(ohm cm)
Coating# available
now1/soon2
Article Number
(WebShop)
PrimeFZ-Si3(100)double-side320 ± 1010000 - 100000 190 / 190WFA30320100X1718SNN1
PrimeFZ-Si3(100)one-side380 ± 1010000 - 1000000 261 / 261WFD30380105X1719SNN2
Borosilicate3###double-side500 ± 25 399 / 399WGS3050025XX0000SNN1
Borosilicate3###one-side150 ± 25 290 / 290WGV30150250X0000SNN1
PrimeSi + Si3N43(100)double-side381 ± 25Boron1 - 1050 nm32 / 32WNA30381250B1314S051
PrimeSi + Si3N43(100)double-side381 ± 25Boron1 - 10150 nm30 / 30WNA30381250B1314S151
PrimeSi + Si3N43(100)double-side381 ± 25Boron1 - 10500 nm34 / 34WNA30381250B1314S501
PrimeSi + Si3N43(100)double-side381 ± 25Boron1 - 10500 nm15 / 15WNA30381250B1314S502
PrimeSi + Si3N43(100)double-side381 ± 25Boron1 - 101000 nm19 / 19WNA30381250B1314SXX2
Quartz3Y-Cutdouble-side500 ± 25 10 / 10WQB30500250XXXXXSNN1
Quartz3Z-Cutdouble-side200 ± 25 14 / 64WQC30200250X0000SNN1
Quartz3Z-Cutdouble-side1000 ± 25 40 / 40WQC31000250X0000SNN1
Quartz3Z-Cutdouble-side1000 ± 25 53 / 53WQC31000251X0000XNN1
Quartz3Z-Cutdouble-side1000 ± 25 35 / 35WQC31000252X0000XNN1
PrimeCZ-Si3(100)double-side200 ± 25Boron1 - 10 224 / 224WSA30200250B1314SNN1
PrimeCZ-Si3(100)double-side360 ± 25Boron0.001 - 0.005 186 / 186WSA30360250B1050SNN1
PrimeCZ-Si3(100)double-side380 ± 25Boron10 - 20 16 / 16WSA30380250B1424SNN1
PrimeCZ-Si3(100)double-side381 ± 25Boron1 - 10 290 / 1290WSA30381250B1314SNN1
PrimeCZ-Si3(100)double-side381 ± 25Phosphor1 - 10 140 / 140WSA30381250P1314SNN1
PrimeCZ-Si3(100)double-side775 ± 25Boron10 - 20 150 / 150WSA30775250B1424SNN1
PrimeCZ-Si3(100)one-side380 ± 25Arsenic0.001 - 0.01 65 / 65WSD30380250A1011SNN1
PrimeCZ-Si3(100)one-side380 ± 25Boron1 - 50 1900 / 1900WSD30380250B1354SNN1
PrimeCZ-Si3(100)one-side381 ± 20Boron1 - 10 1860 / 1860WSD30381200B1314SNN1
PrimeCZ-Si3(100)one-side381 ± 25Phosphor1 - 10 274 / 274WSD30381250P1314SNN1
PrimeCZ-Si3(100)one-side450 ± 10Boron1 - 20 5 / 5WSD30450100B1324SNN1
PrimeCZ-Si3(100)one-side640 ± 25Phosphor1 - 10 1164 / 1164WSD30640250P1314SNN1
PrimeCZ-Si3(111)one-side380 ± 25Phosphor1 - 10 163 / 163WSF30380250P1314SNN1
TestCZ-Si3(100)one-side381 ± 25Boron1 - 20 575 / 600WSM30381250B1324SNN1
Dummy3CZ-Si3(100)one-side380 ± 25Boron0.001 - 100 575 / 575WSV30380250B1015SNN1
Dummy3CZ-Si3(100)one-side380 ± 25Boron0.001 - 100 1000 / 1000WSV30380250B1015SNN2
Dummy3CZ-Si3(111)one-side420 ± 25Boron0.001 - 1 1750 / 1750WSY30420250B1013XNN1
PrimeSi + SiO2 (dry)3(100)double-side200 ± 2510000 - 100000300 nm0 / 150WTA30200250X1718S301
PrimeSi + SiO2 (dry)3(100)one-side200 ± 25Boron1 - 10300 nm8 / 108WTD30200250B1314S301
PrimeSi + SiO2 (dry)3(100)one-side380 ± 105000 - 50000200 nm107 / 107WTD30380100X5617S201
PrimeSi + SiO2 (dry)3(100)one-side380 ± 25Boron1 - 10100 nm95 / 295WTD30380250B1314S101
Fused Silica3###double-side320 ± 10 32 / 32WUA30320100X0000SNN1
Fused Silica3###double-side380 ± 20 0 / 125WUA30380200X0000SNN1
Fused Silica3###double-side500 ± 25 203 / 203WUS30500250X0000SNN2
Fused Silica3###double-side500 ± 25 25 / 25WUS30500250X0000SNN4
Fused Silica3###double-side1000 8 / 8WUS31000000X0000SNN1
Fused Silica3###double-side1000 ± 25 110 / 110WUS31000250X0000SNN1
PrimeSi + SiO2 (wet)3(100)one-side380 ± 25Boron1 - 1090 nm25 / 25WWD30380250B1314S092
PrimeSi + SiO2 (wet)3(100)one-side380 ± 25Boron1 - 10300 nm164 / 164WWD30380250B1314S301
PrimeSi + SiO2 (wet)3(100)one-side380 ± 25Boron1 - 101000 nm195 / 195WWD30380250B1314SXX1
PrimeSi + SiO2 (wet)3(100)one-side381 ± 25Boron1 - 103000 nm40 / 40WWD30381250B1314SXX1
PrimeCZ-Si3(111)one-side380 ± 15Boron0.001 - 0.005 0 / 15(5)WSF30380150B1050SNN#
PrimeCZ-Si3(100)double-side450 ± 20Phosphor20 - 50 0 / 100(5)WSA30450200P2454SNN#
PrimeCZ-Si3(100)one-side380 ± 150.001 - 0.005 0 / 191(5)WSD30380150X1050SNN#
PrimeCZ-Si3(100)one-side430 ± 25Phosphor20 - 50 0 / 11(5)WSD30430250P2454SNN#
PrimeCZ-Si3(111)none240 ± 10Phosphor15 - 20 0 / 20(5)WSI30240100P1424SNN#
PrimeCZ-Si3(111)double-side1050 - 100 0 / 5(5)WSC30105000X0015SNN#
PrimeFZ-Si3(111)double-side380 ± 1010000 - 1000000 0 / 181(5)WFC30380105X1719SNN#
PrimeFZ-Si3(100)one-side380 ± 1010000 - 1000000 0 / 91(5)WFD30380105X1719SNN#
Interested in an offer? Please send us an e-mail with the article numbers(s) (20-digit code in the right column of the table above) and number to info@microchemicals.com
4 Inch Silicon, Quartz, Fused Silica and Glass Wafers
Qual.MaterialSize
(inch)
Orien-
tation
PolishedThick-
ness (μm)
DopingResistivity
(ohm cm)
Coating# available
now1/soon2
Article Number
(WebShop)
PrimeFZ-Si4(100)double-side200 ± 1010000 - 1000000 486 / 486WFA40200105X1719XNN1
PrimeFZ-Si4(100)double-side280 ± 10Boron2000 - 8000 250 / 250WFA40280100B2686SNN1
PrimeFZ-Si4(100)double-side290 ± 10Boron2000 - 8000 2 / 2WFA40290100B2686SNN1
PrimeFZ-Si4(100)double-side400 ± 10Phosphor3000 - 1000000 0 / 93WFA40400105P3619SNN1
PrimeFZ-Si4(100)double-side500 ± 15Boron3000 - 100000 55 / 55WFA40500150B3618SNN1
PrimeFZ-Si4(100)double-side525 ± 1010000 - 100000 446 / 446WFA40525105X1718XNN1
PrimeFZ-Si4(100)double-side525 ± 1020000 - 100000 56 / 56WFA40525105X2718SNN1
PrimeFZ-Si4(111)double-side300 ± 2510000 - 100000 77 / 77WFC40300250X1718SNN1
PrimeFZ-Si4(111)double-side525 ± 15Phosphor2000 - 1000000 52 / 52WFC40525155P2619SNN1
PrimeFZ-Si4(111)one-side300 ± 1510000 - 1000000 171 / 171WFF40300155X1719SNN1
Borosilicate4###double-side175 ± 20 147 / 147WGS40175200X0000SNN1
Borosilicate4###double-side200 ± 20 147 / 147WGS40200200X0000SNN2
Borosilicate4###double-side500 ± 25 25 / 25WGS40500250X0000SNN6
Borosilicate4###double-side500 ± 25 407 / 407WGS40500250XXXXXSNN1
Borosilicate4###double-side700 ± 20 115 / 115WGS40700200X0000SNN2
Borosilicate4###double-side900 ± 30 348 / 348WGS40900300X0000SNN1
Borosilicate4###double-side1000 ± 20 252 / 252WGS41000200X0000SNN1
Borosilicate4###double-side2000 ± 25 130 / 130WGS42000250X0000SNN1
Borosilicate4###one-side700 ± 20 143 / 143WGV40700200X0000SNN1
PrimeSi + Si3N44(100)double-side200 ± 10Boron1 - 1060 nm20 / 70WNA40200105B1314S061
PrimeSi + Si3N44(100)double-side200 ± 10Boron1 - 10200 nm16 / 16WNA40200105B1314S202
PrimeSi + Si3N44(100)double-side260 ± 1010000 - 10000080 nm23 / 23WNA40260100X1718S081
PrimeSi + Si3N44(100)double-side380 ± 15Boron1 - 1050 nm7 / 7WNA40380155B1314S051
PrimeSi + Si3N44(100)double-side380 ± 15Boron1 - 1070 nm48 / 48WNA40380155B1314S071
PrimeSi + Si3N44(100)double-side380 ± 15Boron1 - 10150 nm44 / 44WNA40380155B1314S151
PrimeSi + Si3N44(100)double-side380 ± 15Boron1 - 10400 nm18 / 18WNA40380155B1314S401
PrimeSi + Si3N44(100)double-side380 ± 15Boron1 - 101000 nm54 / 54WNA40380155B1314SXX1
PrimeSi + Si3N44(100)double-side525 ± 15Boron1 - 1030 nm6 / 6WNA40525155B1314S031
PrimeSi + Si3N44(100)double-side525 ± 15Boron1 - 1080 nm25 / 25WNA40525155B1314S081
PrimeSi + Si3N44(100)double-side525 ± 15Boron1 - 10120 nm25 / 25WNA40525155B1314S121
PrimeSi + Si3N44(100)double-side525 ± 15Boron1 - 10500 nm18 / 68WNA40525155B1314S501
PrimeSi + Si3N44(100)double-side525 ± 25Boron1 - 1040 nm11 / 11WNA40525255B1314S041
PrimeSi + Si3N44(100)double-side525 ± 25Boron1 - 10300 nm55 / 55WNA40525255B1314S301
PrimeSi + Si3N44(100)double-side525 ± 25Boron1 - 10450 nm9 / 9WNA40525255B1314S451
PrimeSi + Si3N44(100)one-side325 ± 25Boron1 - 1080 nm25 / 25WND40325250B1314S081
Dummy3Si + Si3N44(100)double-side500 ± 2550 nm10 / 10WNS40500250X0000S051
Quartz4X-Cutdouble-side200 ± 25 100 / 100WQA40200250XXXXXSNN1
Quartz4Z-Cutdouble-side1500 ± 50 0 / 50WQC41500500X0000SNN1
Quartz4ST-Cutdouble-side500 ± 25 18 / 18WQL40500250X0000SNN1
Dummy3CZ-Si4###one-side500 ± 50Boron0.001 - 100 320 / 1320WS440500500B1015XNN1
PrimeCZ-Si4(100)double-side100 ± 10Boron0.001 - 0.01 80 / 380WSA40100105B1011SNN1
PrimeCZ-Si4(100)double-side100 ± 10Boron0.001 - 0.01 73 / 73WSA40100105B1011SNN2
PrimeCZ-Si4(100)double-side100 ± 20Boron0.001 - 0.01 630 / 630WSA40100205B1011SNN1
PrimeCZ-Si4(100)double-side185 ± 10Boron1 - 10 362 / 362WSA40185105B1314SNN1
PrimeCZ-Si4(100)double-side200 ± 10Boron1 - 10 0 / 500WSA40200105B1314SNN1
PrimeCZ-Si4(100)double-side200 ± 25Boron1 - 10 100 / 100WSA40200250B1314SNN1
PrimeCZ-Si4(100)double-side300 ± 5Phosphor2 - 10 67 / 67WSA40300053P2314SNN1
PrimeCZ-Si4(100)double-side300 ± 5Phosphor2 - 10 3 / 3WSA40300055P2314SNN1
PrimeCZ-Si4(100)double-side300 ± 5Phosphor2 - 10 73 / 73WSA40300055P2314SNN2
PrimeCZ-Si4(100)double-side300 ± 25Phosphor0.1 - 1 227 / 227WSA40300250P1213SNN1
PrimeCZ-Si4(100)double-side300 ± 25Phosphor0.02 - 0.05 172 / 172WSA40300250P2151SNN1
PrimeCZ-Si4(100)double-side380 ± 15Boron1 - 10 355 / 355WSA40380155B1314SNN2
PrimeCZ-Si4(100)double-side380 ± 15Boron1 - 10 225 / 225WSA40380155B1314SNN3
PrimeCZ-Si4(100)double-side380 ± 15Boron20 - 100 17 / 17WSA40380155B2415SNN1
PrimeCZ-Si4(100)double-side400 ± 15Boron0.1 - 1 200 / 200WSA40400155B1213SNN1
PrimeCZ-Si4(100)double-side400 ± 25Phosphor1 - 10 90 / 90WSA40400250P1314SNN1
PrimeCZ-Si4(100)double-side525 ± 15Boron1 - 10 8 / 508WSA40525155B1314SNN1
PrimeCZ-Si4(100)double-side525 ± 15Boron1 - 10 10 / 10WSA40525155B1314SNN2
PrimeCZ-Si4(100)double-side525 ± 25Boron0.1 - 1 238 / 238WSA40525250B1213SNN1
PrimeCZ-Si4(100)double-side525 ± 25Phosphor2 - 10 408 / 408WSA40525255P2314SNN1
PrimeCZ-Si4(100)double-side600 ± 25Phosphor1 - 10 80 / 80WSA40600250P1314SNN1
PrimeCZ-Si4(100)double-side800 ± 25Boron1 - 10 48 / 248WSA40800250B1314SNN1
PrimeCZ-Si4(100)double-side1000 ± 25Boron1 - 50 0 / 150WSA41000250B1354SNN1
PrimeCZ-Si4(100)double-side1500 ± 25Boron1 - 10 177 / 177WSA41500250B1314SNN1
PrimeCZ-Si4(111)double-side525 ± 25Boron0.1 - 1 290 / 290WSC40525250B1213SNN1
PrimeCZ-Si4(100)one-side300 ± 25Boron1 - 10 10 / 10WSD40300250B1314SNN1
PrimeCZ-Si4(100)one-side300 ± 25Phosphor1 - 10 46 / 46WSD40300250P1314SNN1
PrimeCZ-Si4(100)one-side325 ± 25Boron1 - 10 249 / 249WSD40325250B1314SNN1
PrimeCZ-Si4(100)one-side525 ± 15Arsenic0.001 - 0.005 66 / 366WSD40525150A1050SNN1
PrimeCZ-Si4(100)one-side525 ± 15Boron10 - 20 100 / 100WSD40525155B1424SNN1
PrimeCZ-Si4(100)one-side525 ± 20Boron1 - 20 29 / 29WSD40525205B1324SNN1
PrimeCZ-Si4(100)one-side525 ± 20Boron1 - 20 496 / 496WSD40525205B1324SNN2
PrimeCZ-Si4(100)one-side525 ± 25Boron0.001 - 0.005 28 / 228WSD40525250B1050SNN1
PrimeCZ-Si4(100)one-side525 ± 25Boron1 - 10 1068 / 1068WSD40525250B1314SNN2
PrimeCZ-Si4(100)one-side525 ± 25Boron1 - 10 345 / 345WSD40525250B1314SNN4
PrimeCZ-Si4(100)one-side525 ± 25Boron1 - 10 0 / 325WSD40525250B1314SNN5
PrimeCZ-Si4(100)one-side525 ± 25Boron5 - 10 0 / 500WSD40525250B5314SNN1
PrimeCZ-Si4(100)one-side525 ± 25Phosphor0.01 - 0.1 161 / 161WSD40525250P1112SNN1
PrimeCZ-Si4(100)one-side525 ± 25Phosphor0.1 - 1 270 / 270WSD40525250P1213SNN1
PrimeCZ-Si4(100)one-side525 ± 25Phosphor1 - 10 190 / 190WSD40525250P1314XNN1
PrimeCZ-Si4(100)one-side525 ± 25Phosphor1 - 10 143 / 343WSD40525250P1314XNN2
PrimeCZ-Si4(100)one-side2000 ± 25Boron1 - 20 206 / 206WSD42000250B1324SNN1
PrimeCZ-Si4(100)one-side3000 ± 25Boron1 - 20 0 / 175WSD43000250B1324SNN1
PrimeCZ-Si4(110)one-side525 ± 25Boron1 - 10 168 / 168WSE40525250B1314SNN1
PrimeCZ-Si4(111)one-side450 ± 250.01 - 0.05 173 / 173WSF40450250X1151SNN1
PrimeCZ-Si4(111)one-side525 ± 25Boron1 - 10 798 / 798WSF40525250B1314SNN2
TestCZ-Si4(100)one-side525 ± 25Phosphor1 - 20 1075 / 1075WSM40525250P1324XNN1
TestCZ-Si4(100)one-side525 ± 25Boron1 - 10 2140 / 2140WSM4052525XB1314SNN1
TestCZ-Si4(100)one-side625 ± 25Boron1 - 10 200 / 200WSM4062525XB1314SNN1
Dummy3CZ-Si4(111)double-side500 ± 25Phosphor5 - 100 200 / 200WSU40500250P5315XNN1
Dummy3CZ-Si4(100)one-side325 ± 25Boron1 - 10 23 / 23WSV40325250B1314SNN1
Dummy3CZ-Si4(100)one-side500 ± 50Boron0.001 - 100 682 / 682WSV40500500B1015XNN1
Dummy3CZ-Si4(100)one-side500 ± 50Boron0.001 - 100 550 / 550WSV4050050XB1015XNN1
Dummy3CZ-Si4(100)one-side625 ± 25Boron1 - 10 25 / 25WSV40625250B1314SNN1
PrimeSi + SiO2 (dry)4(100)double-side525 ± 2510000 - 100000100 nm13 / 13WTA40525250X1718S101
PrimeSi + SiO2 (dry)4(100)one-side525 ± 20Boron0.001 - 0.005290 nm0 / 390WTD40525205B1050S291
PrimeSi + SiO2 (dry)4(100)one-side525 ± 20Boron0.001 - 0.005290 nm50 / 50WTD40525205B1050S293
PrimeSi + SiO2 (dry)4(100)one-side525 ± 25Arsenic0.001 - 0.005200 nm73 / 73WTD40525250A1050S201
PrimeSi + SiO2 (dry)4(100)one-side525 ± 25Boron0.001 - 0.00590 nm86 / 86WTD40525250B1050S091
PrimeSi + SiO2 (dry)4(100)one-side525 ± 25Boron0.001 - 0.005280 nm400 / 400WTD40525250B1050S281
PrimeSi + SiO2 (dry)4(100)one-side525 ± 25Boron1 - 10100 nm92 / 292WTD40525250B1314S102
PrimeSi + SiO2 (dry)4(100)one-side525 ± 25Boron1 - 10200 nm463 / 463WTD40525250B1314S201
PrimeSi + SiO2 (dry)4(100)one-side525 ± 25Phosphor1 - 10100 nm79 / 79WTD40525250P1314S101
PrimeSi + SiO2 (dry)4(100)one-side525 ± 25Boron0.001 - 0.0190 nm176 / 176WTD40525255B1011S091
TestSi + SiO2 (dry)4(100)one-side525 ± 25Boron0.001 - 0.005280 nm25 / 25WTM40525250B1050S281
Dummy3Si + SiO2 (dry)4(100)one-side525 ± 25Boron0.001 - 0.005280 nm259 / 259WTV40525250B1050S281
Fused Silica4###double-side380 ± 20 236 / 236WUA40380200X0000SNN1
Fused Silica4###double-side500 ± 25 177 / 177WUA40500250X0000SNN1
Fused Silica4###double-side250 ± 25 211 / 211WUS40250250XXXXXSNN1
Fused Silica4###double-side350 ± 25 165 / 165WUS40350250XXXXXXNN1
Fused Silica4###double-side500 ± 25 220 / 220WUS40500250X0000SNN2
Fused Silica4###double-side500 ± 25 139 / 139WUS40500250X0000SNN4
Fused Silica4###double-side1000 ± 25 387 / 387WUS41000250X0000SNN1
Fused Silica4###double-side1000 ± 25 293 / 293WUS41000250X0000SNN2
PrimeSi + SiO2 (wet)4(100)double-side350 ± 1510000 - 100000300 nm17 / 17WWA40350150X1718SNN1
PrimeSi + SiO2 (wet)4(100)double-side525 ± 15Boron1 - 10300 nm65 / 65WWA40525150B1314SNN2
PrimeSi + SiO2 (wet)4(100)double-side525 ± 25Phosphor1 - 105000 nm67 / 67WWA40525250P1314SXX1
PrimeSi + SiO2 (wet)4(100)one-side525 ± 25Arsenic0.001 - 0.005300 nm221 / 221WWD40525250A1050S301
PrimeSi + SiO2 (wet)4(100)one-side525 ± 25Boron1 - 10300 nm481 / 481WWD40525250B1314S302
PrimeSi + SiO2 (wet)4(100)one-side525 ± 25Boron1 - 10500 nm416 / 416WWD40525250B1314S501
PrimeSi + SiO2 (wet)4(100)one-side525 ± 25Boron1 - 101000 nm238 / 238WWD40525250B1314SXX1
PrimeSi + SiO2 (wet)4(100)one-side525 ± 25Boron1 - 101500 nm337 / 337WWD40525250B1314SXX3
PrimeSi + SiO2 (wet)4(100)one-side525 ± 25Boron1 - 102000 nm225 / 225WWD40525250B1314SXX6
PrimeSi + SiO2 (wet)4(100)one-side525 ± 25Boron1 - 105000 nm70 / 70WWD40525250B1314SXX8
PrimeSi + SiO2 (wet)4(100)one-side525 ± 25Phosphor1 - 101000 nm125 / 125WWD40525250P1314SXX1
PrimeSi + SiO2 (wet)4(100)one-side525 ± 25Phosphor1 - 102280 nm50 / 50WWD40525250P1314SXX2
PrimeSi + SiO2 (wet)4(100)one-side525 ± 251000 - 100000300 nm3 / 3WWD40525250X1618S301
PrimeSi + SiO2 (wet)4(100)one-side625 ± 25Phosphor10 - 201000 nm149 / 149WWD40625250P1424SXX1
PrimeSi + SiO2 (wet)4(111)one-side525 ± 25Phosphor1 - 101000 nm1 / 1WWF40525250P1314SXX1
PrimeCZ-Si4(100)double-side300 ± 100.002 - 0.004 0 / 84(5)WSA40300105X2040SNN#
PrimeCZ-Si4(100)double-side100 ± 5Boron0 - 0.01 0 / 25(5)WSA40100055B0011SNN#
PrimeCZ-Si4(100)double-side380 ± 15Phosphor2 - 10 0 / 340(5)WSA40380155P2314SNN#
PrimeCZ-Si4(100)double-side525 ± 25Phosphor1 - 10 0 / 50(5)WSA40525250P1314SNN#
PrimeCZ-Si4(100)double-side1000 ± 25Phosphor0 - 0.005 0 / 15(5)WSA41000250P0050SNN#
PrimeCZ-Si4(100)double-side800 ± 20Boron1 - 10 0 / 145(5)WSA40800200B1314SNN#
PrimeCZ-Si4(110)one-side525 ± 15Boron5 - 8 0 / 100(5)WSE40525155B5383SNN#
XCZ-Si4###525 ± 15Boron1 - 10 0 / 75(5)WSX40525150B1314SNN#
PrimeFZ-Si4(100)double-side300 ± 20Boron1 - 5 0 / 35(5)WFA40300205B1353SNN#
PrimeFZ-Si4(111)one-side300 ± 1510000 - 1000000 0 / 125(5)WFF40300155X1719SNN#
PrimeFZ-Si4(111)double-side300 ± 10Phosphor5000 - 1000000 0 / 298(5)WFC40300105P5619SNN#
PrimeFZ-Si4(100)one-side525 ± 10Boron2000 - 4000 0 / 115(5)WFD40525105B2646SNN#
PrimeFZ-Si4(111)double-side525 ± 15Phosphor2000 - 1000000 0 / 260(5)WFC40525155P2619SNN#
PrimeFZ-Si4(100)double-side300 ± 10Boron150 - 500 0 / 44(5)WFA40300100B1555SNN#
PrimeFZ-Si4(100)one-side525 ± 1010000 - 1000000 0 / 76(5)WFD40525105X1719SNN#
PrimeFZ-Si4(111)double-side525 ± 1020000 - 1000000 0 / 152(5)WFC40525105X2719SNN#
PrimeFZ-Si4(100)double-side400 ± 10Phosphor3000 - 1000000 0 / 150(5)WFA40400105P3619SNN#
PrimeFZ-Si4(100)double-side200 ± 1010000 - 1000000 0 / 100(5)WFA40200105X1719SNN#
Interested in an offer? Please send us an e-mail with the article numbers(s) (20-digit code in the right column of the table above) and number to info@microchemicals.com
5 Inch Silicon, Quartz, Fused Silica and Glass Wafers
Qual.MaterialSize
(inch)
Orien-
tation
PolishedThick-
ness (μm)
DopingResistivity
(ohm cm)
Coating# available
now1/soon2
Article Number
(WebShop)
PrimeCZ-Si5(100)double-side600 ± 15Phosphor1 - 10 153 / 153WSA50600155P1314SNN1
PrimeCZ-Si5(100)one-side525 ± 25Boron1 - 10 221 / 221WSD50525250B1314SNN1
TestCZ-Si5(100)one-side525 ± 25Boron1 - 10 150 / 150WSM50525250B1314SNN1
Dummy3CZ-Si5(100)one-side525 ± 50Phosphor0.001 - 100 225 / 225WSV50525500P1015SNN1
Interested in an offer? Please send us an e-mail with the article numbers(s) (20-digit code in the right column of the table above) and number to info@microchemicals.com
6 Inch Silicon, Quartz, Fused Silica and Glass Wafers
Qual.MaterialSize
(inch)
Orien-
tation
PolishedThick-
ness (μm)
DopingResistivity
(ohm cm)
Coating# available
now1/soon2
Article Number
(WebShop)
PrimeFZ-Si6(100)double-side300 ± 1010000 - 100000 123 / 123WFA60300100X1718SNN1
PrimeFZ-Si6(100)double-side380 ± 1010000 - 100000 113 / 113WFA60380100X1718SNN1
Borosilicate6###double-side700 ± 20 299 / 299WGS60700200X0000SNN1
Borosilicate6###double-side700 ± 20 14 / 14WGS60700200X0000XNN1
Borosilicate6###one-side700 ± 25 112 / 112WGV60700250X0000SNN2
Dummy3CZ-Si6###one-side650 ± 50Boron0.001 - 100 600 / 600WS460650500B1015XNN1
PrimeCZ-Si6(100)double-side381 ± 15Boron1 - 10 500 / 500WSA60381150B1314SNN1
PrimeCZ-Si6(100)double-side400 ± 10Boron10 - 20 46 / 46WSA60400107B1424XNN1
PrimeCZ-Si6(100)double-side525 ± 25Boron1 - 10 105 / 105WSA60525255B1314SNN1
PrimeCZ-Si6(100)double-side675 ± 25Boron1 - 10 538 / 538WSA60675250B1314SNN1
PrimeCZ-Si6(100)one-side675 ± 20Boron1 - 10 95 / 295WSD60675200B1314XNN1
PrimeCZ-Si6(100)one-side675 ± 20Boron100 - 150 77 / 77WSD60675200B1515XNN1
PrimeCZ-Si6(100)one-side675 ± 25Boron1 - 10 391 / 391WSD60675250B1314SNN1
PrimeCZ-Si6(100)one-side675 ± 25Boron1 - 20 75 / 75WSD60675250B1324SNN1
PrimeCZ-Si6(100)one-side675 ± 25Boron1 - 10 100 / 100WSD60675255B1314SNN1
PrimeCZ-Si6(100)one-side1000 ± 25Boron3 - 10 1 / 1WSD61000250B3314SNN1
TestCZ-Si6(100)one-side675 ± 10Boron1 - 10 125 / 125WSM60675100B1314SNN1
TestCZ-Si6(100)one-side675 ± 25Boron1 - 10 413 / 413WSM6067525XB1314SNN1
Dummy3CZ-Si6(100)one-side650 ± 50Phosphor0.001 - 100 150 / 150WSV60650500P1015XNN1
Dummy3CZ-Si6(100)one-side650 ± 500.001 - 100 600 / 600WSV60650500X1015XNN1
Dummy3CZ-Si6(100)one-side650 ± 50Boron0.001 - 100 550 / 550WSV6065050XB1015XNN1
Dummy3CZ-Si6(100)one-side650 ± 50Boron0.001 - 100 266 / 266WSV6065050XB1015XNN2
PrimeSi + SiO2 (dry)6(100)one-side675 ± 25Boron1 - 10100 nm100 / 100WTD60675250B1314S101
Fused Silica6###double-side700 ± 25 70 / 70WUS60700250X0000SNN1
Fused Silica6###double-side1000 ± 25 144 / 144WUS61000250X0000SNN1
Fused Silica6###double-side1000 ± 25 125 / 125WUS61000250X0000SNN2
Fused Silica6###double-side1000 ± 25 133 / 133WUS61000250XXXXXXNN1
Fused Silica6###double-side1000 ± 25 20 / 20WUS61000250XXXXXXNN2
PrimeSi + SiO2 (wet)6(100)one-side675 ± 25Boron1 - 10300 nm240 / 240WWD60675250B1314S301
PrimeSi + SiO2 (wet)6(100)one-side675 ± 25Phosphor1 - 101000 nm20 / 20WWD60675250P1314SXX1
PrimeSi + SiO2 (wet)6(100)one-side675 ± 25Phosphor1 - 101000 nm43 / 43WWD6067525XP1314SXX1
PrimeCZ-Si6(100)one-side625 ± 10Boron12 - 18 0 / 12(5)WSD60625105B1414SNN#
PrimeCZ-Si6(100)one-side675 ± 10Phosphor1 - 10 0 / 1000(5)WSD60675100P1314SNN#
PrimeFZ-Si6(111)double-side1000 ± 106000 - 1000000 0 / 3(5)WFC61000106X6619SNN#
PrimeFZ-Si6(111)double-side300 ± 10Phosphor6000 - 1000000 0 / 11(5)WFC60300106P6619SNN#
PrimeFZ-Si6(100)one-side425 ± 15Phosphor5000 - 6300 0 / 231(5)WFD60425155P5666SNN#
PrimeCZ-Si6(100)one-side508 ± 16Arsenic0 - 0.005 0 / 4150(5)WSD6050816XA0050SNN§
PrimeCZ-Si6(111)one-side675 ± 21Boron10 - 20 0 / 1600(5)WSF6067521XB1424SNN§
PrimeCZ-Si6(111)one-side675 ± 21Boron5 - 15 0 / 500(5)WSF6067521XB5314SNN§
PrimeCZ-Si6(111)one-side675 ± 21Boron4.5 - 6.5 0 / 456(5)WSF6067521XB4363SNN§
PrimeCZ-Si6(111)one-side525 ± 16Boron3 - 5 0 / 244(5)WSF6052516XB3353SNN§
PrimeCZ-Si6(111)one-side625 ± 160.008 - 0.017 0 / 225(5)WSF6062516XX8011SNN§
PrimeCZ-Si6(100)one-side625 ± 26Boron7 - 17 0 / 48(5)WSD6062526XB7314SNN§
PrimeFZ-Si6(111)one-side625 ± 16Phosphor50 - 80 0 / 72(5)WFF6062516XP5484SNN§
PrimeFZ-Si6(100)one-side675 ± 26Boron700 - 1300 0 / 48(5)WFD6067526XB7516SNN§
Interested in an offer? Please send us an e-mail with the article numbers(s) (20-digit code in the right column of the table above) and number to info@microchemicals.com
8 Inch Silicon, Quartz, Fused Silica and Glass Wafers
Qual.MaterialSize
(inch)
Orien-
tation
PolishedThick-
ness (μm)
DopingResistivity
(ohm cm)
Coating# available
now1/soon2
Article Number
(WebShop)
Borosilicate8###double-side1250 ± 25 58 / 58WGS81250250X0000SNN2
PrimeCZ-Si8(100)double-side625 ± 250.001 - 1000 700 / 700WSA80625255X1016SNN1
PrimeCZ-Si8(100)double-side675 ± 250.001 - 1000 150 / 150WSA80675255X1016SNN1
PrimeCZ-Si8(100)one-side675 ± 250.001 - 1000 524 / 524WSD80675255X1016SNN1
PrimeCZ-Si8(100)one-side675 ± 750.001 - 1000 125 / 125WSD80675755X1016SNN1
PrimeCZ-Si8(100)one-side725 ± 25Boron1000 - 10000 29 / 29WSD80725250B1617XNN1
TestCZ-Si8(100)one-side725 ± 25Boron1 - 100 194 / 194WSM80725250B1315SNN1
TestCZ-Si8(100)one-side725 ± 25Boron1 - 100 1000 / 1000WSM80725250B1315XNN1
Dummy3CZ-Si8(100)double-side650 ± 50Boron0.001 - 1000 250 / 250WSS80650500B1016XNN1
Dummy3CZ-Si8(100)one-side650 ± 50Boron0.001 - 1000 750 / 750WSV80650500B1016XNN1
Dummy3CZ-Si8(100)one-side650 ± 50Boron1 - 1000 700 / 700WSV80650500B1316XNN1
Dummy3CZ-Si8(100)one-side725 ± 50Boron1 - 1000 375 / 375WSV80725500B1316XNN1
Dummy3CZ-Si8(100)one-side750 ± 250.001 - 100 480 / 480WSV80750250X1015SNN1
Fused Silica8###double-side700 ± 25 26 / 26WUS80700250X0000SNN2
Interested in an offer? Please send us an e-mail with the article numbers(s) (20-digit code in the right column of the table above) and number to info@microchemicals.com
12 Inch Silicon, Quartz, Fused Silica and Glass Wafers
Qual.MaterialSize
(inch)
Orien-
tation
PolishedThick-
ness (μm)
DopingResistivity
(ohm cm)
Coating# available
now1/soon2
Article Number
(WebShop)
Dummy3CZ-Si12###double-side750 ± 250.001 - 1000 25 / 25WS5A0750250X1016SNN1
Dummy3CZ-Si12(100)double-side755 ± 500.001 - 10000 349 / 349WSSA0755500X1017XNN1
Dummy3CZ-Si12(100)double-side775 ± 25Boron1 - 100 350 / 350WSSA0775250B1315SNN1
Interested in an offer? Please send us an e-mail with the article numbers(s) (20-digit code in the right column of the table above) and number to info@microchemicals.com
Rectangular Cut Wafer Pieces
Qual.MaterialSize
(mm)
Orien-
tation
PolishedThick-
ness (μm)
DopingResistivity
(ohm cm)
Coating# available
now1/soon2
Article Number
(WebShop)
Borosilicate5 x 5 mm###double-side700 880 / 880W9GS0050050700NNNNX1
Borosilicate10 x 10 mm###double-side1000 590 / 590W9GS0100101000NNNNX1
Borosilicate20 x 20 mm###double-side500 1264 / 1264W9GS0200200500NNNNX1
Borosilicate32 x 24 mm###double-side200 88 / 88W9GS0320240200NNNNX1
Borosilicate50 x 50 mm###double-side1000 395 / 395W9GS0500501000NNNNX1
Borosilicate100 x 100 mm###double-side1000 125 / 125W9GS1001001000NNNNX1
Quartz49 x 49 mmX-Cutdouble-side170 70 / 70W9QA0490490170NNNNX1
Quartz30 x 30 mmZ-Cutdouble-side700 236 / 236W9QC0300300700NNNNX1
PrimeCZ-Si10 x 10 mm(100)one-side525Boron1 - 20 1242 / 1242W9SD0100100525NNNNB1
PrimeCZ-Si25 x 10 mm(100)one-side525Boron1 - 20 550 / 550W9SD0250100525NNNNB1
PrimeCZ-Si25 x 25 mm(100)one-side500Boron1 - 20 520 / 520W9SD0250250500NNNNB1
PrimeCZ-Si50 x 10 mm(100)one-side525Boron1 - 20 376 / 376W9SD0500100525NNNNB1
PrimeCZ-Si100 x 100 mm(100)one-side625Boron1 - 20 129 / 129W9SD1001000625XXXNB1
PrimeSi + SiO2 (dry)10 x 10 mm(100)one-side525Boron1 - 10200 nm1008 / 1008W9TD01001005250200B1
PrimeSi + SiO2 (dry)25 x 25 mm(100)one-side525Boron1 - 10200 nm5 / 505W9TD02502505250200B1
PrimeSi + SiO2 (dry)100 x 100 mm(100)one-side525Boron1 - 10200 nm34 / 34W9TD10010005250200B2
Fused Silica25 x 25 mm###double-side700 1600 / 9600W9UA0250250700NNNNX1
Fused Silica90 x 20 mm###one-side1000 30 / 30W9UD0900201000NNNNX1
Fused Silica8 x 7 mm###double-side170 0 / 800W9US0080070170NNNNX1
Fused Silica10 x 10 mm###double-side170 1000 / 1000W9US0100100170NNNNX1
Fused Silica10 x 10 mm###double-side500 1360 / 1360W9US0100100500NNNNX1
Fused Silica10 x 10 mm###double-side1000 850 / 850W9US0100101000NNNNX1
Fused Silica10 x 20 mm###double-side500 1660 / 1660W9US0100200500NNNNX1
Fused Silica15 x 11 mm###double-side1000 180 / 180W9US0150111000NNNNX1
Fused Silica20 x 20 mm###double-side250 2000 / 2000W9US0200200250NNNNX1
Fused Silica20 x 20 mm###double-side700 1101 / 1101W9US0200200700NNNNX1
Fused Silica25 x 25 mm###double-side500 100 / 600W9US0250250500NNNNX1
Fused Silica30 x 30 mm###double-side200 0 / 247W9US0300300200NNNNX1
Fused Silica30 x 30 mm###double-side500 0 / 249W9US0300300500NNNNX1
Fused Silica30 x 30 mm###double-side1000 0 / 100W9US0300301000NNNNX1
Fused Silica35 x 35 mm###double-side700 175 / 175W9US0350350700NNNNX1
Fused Silica50 x 50 mm###double-side300 108 / 108W9US0500500300NNNNX1
Fused Silica50 x 50 mm###double-side2000 0 / 169W9US0500502000NNNNX1
Fused Silica100 x 100 mm###double-side160 230 / 230W9US1001000160NNNNX1
Fused Silica100 x 100 mm###double-side200 50 / 50W9US1001000200NNNNX2
PrimeSi + SiO2 (wet)100 x 100 mm(100)one-side525Boron1 - 101000 nm5 / 5W9WD10010005251000B1
Interested in an offer? Please send us an e-mail with the article numbers(s) (20-digit code in the right column of the table above) and number to info@microchemicals.com
1 available when this list has been revised
2 available + ordered (= available in typically few weeks)
3 Wider specified, rather cheap wafers for e. g. resist coating tests or start-up experiments for new litho-processes.
4 prices subject to change; while stocks last.
5 possibly available on demand within approx. 1 - 2 weeks.

 
       
We try to revise this stock list daily or weekly, but we cannot guarantee that it's always up-to-date.